BEND-INDUCED LOSSES IN A SINGLE-MODE MICROSTRUCTURED FIBER WITH A LARGE CORE

Annotation
A study of bend-induced losses in a silica-based single-mode microstructured fiber with a core diameter ranging from 20 to 35 microns and increased relative air content in the holey cladding has been conducted. With the use of the equivalent step-index profile method in approximation of waveguide parameters of microstructured fiber (normalized frequency and normalized transverse attenuation constant) the effect of bending on the spectral position of the fundamentalmode short-wavelength leakage boundary has been analyzed. Upon measurement of spectral characteristics of attenuation in the considered fibers good accordance of numerical and experimental data has been found out. It is shown that increase of the air content in the holey cladding leads to expansion of the mentioned boundary to lower wavelengths for the value from 150 to 800 nm depending on the core size and bending conditions. A single-transverse-mode propagation is achieved on fiber length of 5-10 meters due to a substantial difference in losses of fundamental and higher-order guided modes attained by bending. Optical losses in all studied samples are less than 10 dB/km at the wavelength λ = 1550 nm. The results of the study can be applied in the design of high-power laser systems having such basic requirements as a relatively large mode spot and high beam quality.
Keywords
Постоянный URL
Articles in current issue
- METHODS AND TECHNIQUE FOR THERMOPOWER AND ELECTRICAL CONDUCTIVITY MEASUREMENTS OF THERMOELECTRIC MATERIALS AT HIGH TEMPERATURES
- STUDY OF BIREFRINGENCE INFLUENCE ON IMAGE QUALITY OF PHOTOLITHOGRAPHY SYSTEMS IN VIEW OF PARTIALLY-COHERENT LIGHT SOURCE
- EDGE EFFECT MODELING AND STUDY FOR THREE-CHIP RGB LIGHT-EMITTING DIODES
- NON-INTRUSIVE GAS-PHASE THERMOMETRY FOR INDUSTRIAL OXY-FUEL BURNERS
- A SIGNAL ENHANCED PORTABLE RAMAN PROBE FOR ANESTHETIC GAS MONITORING
- COMPENSATION OF OUTPUT SIGNAL TEMPERATURE DEPENDENCE IN HOMODYNE DEMODULATION TECHNIQUE FOR PHASE FIBER-OPTIC SENSORS
- STUDY OF REFLECTION COEFFICIENT DISTRIBUTION FOR ANTI-REFLECTION COATINGS ON SMALL-RADIUS OPTICAL PARTS
- PROTECTIVE COATINGS OF FIBER BRAGG GRATING FOR MINIMIZING OF MECHANICAL IMPACT ON ITS WAVELENGTH CHARACTERISTICS
- TWO-MOTOR ELEVATION DRIVE OF THE PRECISION TWIN TELESCOPE
- ELECTRON DIFFRACTION STUDY OF GRAPHENE LAYERS STRUCTURE ON CONDUCTIVE AND SEMI-INSULATING 6H-SIC (0001) SUBSTRATES
- SAXSEV 2.1 CROSS-PLATFORM APPLICATION FOR DATA ANALYSIS OF SMALL-ANGLE X-RAY SCATTERING FROM POLYDISPERSE SYSTEMS
- NEW BIOTESTING METHOD WITH THE APPLICATION OF MODERN IMPEDANCE TECHNOLOGIES
- ENERGY CONSUMPTION MONITORING OF SMART GRID BASED ON SEMANTIC STREAM DATA ANALYSIS
- METHODS OF POLYMODAL INFORMATION TRANSMISSION
- FREQUENCY OPTIMIZATION FOR SECURITY MONITORING OF COMPUTER SYSTEMS
- MODEL OF PROVIDING WITH DEVELOPMENT STRATEGY FOR INFORMATION TECHNOLOGIES IN AN ORGANIZATION
- METHODS FOR SOLVING LINEAR PROGRAMMING PROBLEMS WITH ADDITIONAL RESTRICTIONS TO THE PARTICULAR VARIABLES
- INTERVAL ADDITIVE PIECEWISE POLYNOMIAL TIME OPERATION MODEL OF HUMAN-OPERATOR IN A QUASI-FUNCTIONAL ENVIRONMENT
- OBLIQUE SHOCK WAVE REFLECTION FROM THE WALL
- OPTIMIZATION OF THE COVERAGE ZONE FOR A CELLULAR NETWORK BASED ON MATHEMATICAL PROGRAMMING
- INTERFERENCE OF COUNTERPROPAGATING SHOCK WAVES
- COMPACT REPRESENTATION OF THE PRIORITY MATRIX WITH HIGH DIMENSIONALITY
- MERIDIONAL COMA OF NEGATIVE ANASTIGMATIC LENSES AT THE FINAL POSITION OF AN OBJECT
- LUMINESCENCE OF CADMIUM SULFIDE QUANTUM DOTS IN FLUOROPHOSPHATE GLASSES