Annotation
Modern nickel-based superalloys contain high concentrations of rhenium that allows the improvement of their creep strength. The high levels of rhenium, however, results in the formation of topologically close-packed phases (TCP) which have a negative influence on its properties. The addition of ruthenium was found to reduce the precipitation of nano-sized TCP phases, but the reasons have not been established. In this paper, by using an ab-initio approach, we studied the effect of rhenium and ruthenium on the structural properties of Ni matrix as well as the TCP phases. We demonstrate that Cr, Mo and W are the most effective additions to provoke the formation of TCP phases, whereas ruthenium has a destabilizing effect.
Keywords
Постоянный URL
Articles in current issue
- In Memoriam: Alexander Ivanovskii, innovative researcher and science manager in computational materials science of advanced inorganic materials
- Scientific activities of Professor A.L. Ivanovskii in bibliometric indeces
- Chlorgraphynes: formation path, structure and electronic properties
- Electronic structure and stabilization of C60 fullerene encapsulating actinide atom
- Boron-doped anatase: electronic band structure, boron atom locations and magnetic state
- Electronic properties of MoS2 monolayer and related structures
- Cubic ordered modification of titanium monoxide with structural vacancies on metal and nonmetal sublattices: electronic structure and stability
- Relations between activation energies for nucleation and of growth of crystals
- Synthesis and photocatalytic activity of quasi-one-dimensional (1-D) solid solutions Ti1-xMxO2-2x/2 (M(III)= Fe(III), Ce(III), Er(III), Tb(III), Eu(III), Nd(III) and Sm(III), 0≤x≤0.1)
- Effect of high pressures and high temperatures on structural and magnetic characteristics of nanostructured solid solutions Zn1-xFexO
- Rhenium carbides prepared by thermobaric treatment of nanosized precursors
- A facile route of coupling of ZnO nanorods by CdS nanoparticles using chemical bath deposition
- Synthesis and study of nanosized biomaterials based on hydroxyapatite
- Adsorption capacity of water-oxidized lanthanum-doped aluminum alloy powder
- Introduction of scandium, zirconium and hafnium into aluminum alloys. Dispersion hardening of intermetallic compounds with nanodimensional particles