Journal
ИЗВЕСТИЯ ВЫСШИХ УЧЕБНЫХ ЗАВЕДЕНИЙ «ПРИБОРОСТРОЕНИЕ»
UDK621.315.592; 621.382.002
Issue:10 (51)
Download PDF0 Kbyte
The influence of laser microstructurization of mono-crystal silicon on morphological and optical properties of the irradiated zones is considered. There are very compound changes of structure on the surface of irradiated zone of silicon, accompanied the morphotropy of silicon and the formation of nanoclusters. At the same time the change of transmission coefficient of irradiated zone of silicon surface was found, that means the change of optical properties of silicon.